Fabrication of microstructures with a femtosecond laser

Jure Javornik, 2022, master's thesis

Description: The master's thesis describes a system for processing optical fibres and glass capillaries, built as an extension of an existing fs laser system. It describes the method of generating ultrashort laser pulses and the theory of their interaction with the processed material. It then covers the fabrication of sensors using an open microcell made from a glass capillary on the processing system. The spectral responses of the sensors and the measurements of their mechanical properties are given. Microfluidic channels, microscrews and microresonators made on the tip of an optical fibre are presented. We also show that mirrors can be inscribed in the core of an optical fibre with an fs laser by inducing a local change in the refractive index. The optical and mechanical properties of the inscribed mirrors were measured at different pulse energies and mirror configurations. Two practical applications of the inscribed mirrors are presented.
Keywords: Ultrashort pulses, femtosecond laser, microstructures, inscribed mirrors, microcell
Published in DKUM: 24.10.2022
Full text (5,20 MB)